| MATERIA | DEPOSITIO technologiae | DENSITAS g/cm3 | Sp3% | DURITIA GPa | FRICTIONE COEFFICIENT |
| DIAMOND | NATURAL | 3.52 | 100 | 100 | 0.02~ 0.10 |
| a-C | RAPIDUS | 1.9~2.4 | 25 | 11~24 | 0.10~0.15 |
| a-C:H:M | REAGENS SUTTERING | 1.9~2.4 |
| 10~20 | 0.10~0.20 |
| a-C:H | RF SUTTERING | 1.57~1.70 |
| 16~40 | 0.02~0.47 |
| a-C,a-C:H | ION TRABES | 1.8~3.5 |
| 32~75 | 0.06~0.19 |
| ta-C | MAGNET FILTER | 2.8~3.0 | 85~95 | 40~80 | 0.04~0.14 |
| Ta-C | PLD | 2.4 | 85~95 | 40~80 | 0.03~0.15 |
| NAMI DIAMOND | PLD | 2.9~3.5 | 75 | 80~100 |
|